Hardness, Brinell HB
297 [-] at 20 °C
Tensile strength Rm
690 MPa at 20 °C
Yield strength YS
485 MPa at 20 °C
Element
Weight %
Comment
60.87 - 69.35 %
26 - 29 %
3.5 - 5.2 %
1 - 2.5 %
0.15 - 0.35 %
Processing history
annealed
This material data has been provided by MetalInfo.