Customize your search with filters
Do you have any questions?
Reduction of area Z
40 % at 20 °C
Tensile strength Rm
485 MPa at 20 °C
Yield strength YS
380 MPa at 20 °C
Element
Weight %
Comment
64.77 - 68.5 %
28 - 30 %
3.5 - 4.2 %
0 - 0.02 %
0 - 0.01 %
Processing history
annealed
This material data has been provided by MetalInfo.