General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 40 % Show Material materials with Elongation A50 of 40 % | |
Hardness, Brinell | 23.0 °C | 250 [-] Show Material materials with Hardness, Brinell of 250 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 40 % Show Material materials with Reduction of area of 40 % | |
Tensile strength | 23.0 °C | 750 MPa Show Material materials with Tensile strength of 750 MPa | |
Yield strength Rp0.2 | 23.0 °C | 430 MPa Show Material materials with Yield strength Rp0.2 of 430 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.02 % Show Material materials with Carbon of 0.02 % |
Chromium | 24 - 25 % Show Material materials with Chromium of 24 - 25 % |
Manganese | 2 - 4 % Show Material materials with Manganese of 2 - 4 % |
Molybdenum | 7 - 8 % Show Material materials with Molybdenum of 7 - 8 % |
Nickel | 21 - 23 % Show Material materials with Nickel of 21 - 23 % |
Nitrogen | 0.45 - 0.55 % Show Material materials with Nitrogen of 0.45 - 0.55 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.5 % Show Material materials with Silicon of 0.5 % |
Sulfur | 5E-3 % Show Material materials with Sulfur of 5E-3 % |