Mechanical
Chemical properties
Property | Value |
---|---|
Carbon | 0.06 % Show Material materials with Carbon of 0.06 % |
Chromium | 20 - 23 % Show Material materials with Chromium of 20 - 23 % |
Iron | 5 % Show Material materials with Iron of 5 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Molybdenum | 8 - 10 % Show Material materials with Molybdenum of 8 - 10 % |
Niobium | 3.15 - 4.5 % Show Material materials with Niobium of 3.15 - 4.5 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |