General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Manganese Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Manganese Steel |
Elongation A50 | 23.0 °C | 20 % Show Material materials with Elongation A50 of 20 % | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Manganese Steel |
Tensile strength | 23.0 °C | 390 MPa Show Material materials with Tensile strength of 390 MPa | |
Yield strength | 23.0 °C | 300 MPa Show Material materials with Yield strength of 300 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.33E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.33E-5 1/K | Typical for Manganese Steel |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Manganese Steel | |
Specific heat capacity | 23.0 °C | 510 - 553 J/(kg·K) Show Material materials with Specific heat capacity of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
Thermal conductivity | 23.0 °C | 14 - 16 W/(m·K) Show Material materials with Thermal conductivity of 14 - 16 W/(m·K) | Typical for Manganese Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.12 % Show Material materials with Carbon of 0.12 % |
Chromium | 0.15 % Show Material materials with Chromium of 0.15 % |
Copper | 0.2 % Show Material materials with Copper of 0.2 % |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % |
Molybdenum | 0.06 % Show Material materials with Molybdenum of 0.06 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Niobium | 8E-3 % Show Material materials with Niobium of 8E-3 % |
Phosphorus | 0.12 % Show Material materials with Phosphorus of 0.12 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |
Titanium | 0.03 % Show Material materials with Titanium of 0.03 % |
Vanadium | 8E-3 % Show Material materials with Vanadium of 8E-3 % |