ASTM A789 Grade S31500 Heat-Treated

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Properties

General

Density ρ

7.8 g/cm³ at 20 °C

Typical for Duplex Stainless Steel

Mechanical

Elastic modulus E

200 GPa at 20 °C

Typical for Duplex Stainless Steel

Elongation A50 A50

30 % at 20 °C

Hardness, Brinell HB

290 [-] at 20 °C

Hardness, Rockwell C HRC

30 [-] at 20 °C

Hardness, Vickers HV

290 [-] at 20 °C

Poisson's ratio ν

0.3 [-] at 20 °C

Typical for Duplex Stainless Steel

Tensile strength Rm

630 MPa at 20 °C

Yield strength YS

440 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1E-5 1/K at 20 °C

Typical for Duplex Stainless Steel

Max service temperature Tmax

300 °C

Typical for Duplex Stainless Steel

Melting point Tm

1375 - 1450 °C

Typical for Duplex Stainless Steel

Specific heat capacity cp

440 - 502 J/(kg·K) at 20 °C

Typical for Duplex Stainless Steel

Thermal conductivity λ

13 - 30 W/(m·K) at 20 °C

Typical for Duplex Stainless Steel

Chemical properties

Element

Weight %

Comment

Cr

18 - 19 %

Ni

4.3 - 5.2 %

Mo

2.5 - 3 %

Si

1.4 - 2 %

Mn

1.2 - 2 %

More

This material data has been provided by ASTM.