Mechanical

PropertyTemperatureValue

Elongation A50

23.0 °C

25 - 35 %

Show Material materials with Elongation A50 of 25 - 35 %

Tensile strength

23.0 °C

490 MPa

Show Material materials with Tensile strength of 490 MPa

Yield strength

23.0 °C

215 MPa

Show Material materials with Yield strength of 215 MPa

Chemical properties

PropertyValue

Carbon

0.02 %

Show Material materials with Carbon of 0.02 %

Chromium

19 - 23 %

Show Material materials with Chromium of 19 - 23 %

Copper

1 - 2 %

Show Material materials with Copper of 1 - 2 %

Manganese

2 %

Show Material materials with Manganese of 2 %

Molybdenum

4 - 5 %

Show Material materials with Molybdenum of 4 - 5 %

Nickel

23 - 28 %

Show Material materials with Nickel of 23 - 28 %

Nitrogen

0.1 %

Show Material materials with Nitrogen of 0.1 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.03 %