ASTM A420 Grade WPL9 Normalized, Normalized and Tempered, Annealed, or Quenched and Tempered

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Typical for Steel

Mechanical

PropertyTemperatureValueComment

Charpy impact energy

23.0 °C

17.6 J

Show Material materials with Charpy impact energy of 17.6 J

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Elongation A50

23.0 °C

18 - 28 %

Show Material materials with Elongation A50 of 18 - 28 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Tensile strength

23.0 °C

435 - 610 MPa

Show Material materials with Tensile strength of 435 - 610 MPa

Yield strength

23.0 °C

315 MPa

Show Material materials with Yield strength of 315 MPa

Chemical properties

PropertyValue

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

Copper

0.75 - 1.25 %

Show Material materials with Copper of 0.75 - 1.25 %

Manganese

0.4 - 1.06 %

Show Material materials with Manganese of 0.4 - 1.06 %

Nickel

1.6 - 2.24 %

Show Material materials with Nickel of 1.6 - 2.24 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Sulfur

0.03 %