See where ASTM A182 Grade F316 Solution-Annealed falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ7.9 - 8.2 g/cm³ at 20 °C
Typical for Austenitic Stainless Steel
Coefficient of thermal expansion
α1.7E-5 - 1.9E-5 1/K at 20 °C
Typical for Austenitic Stainless Steel
Melting point
Tm1375 - 1450 °C
Typical for Austenitic Stainless Steel
Specific heat capacity
cp440 J/(kg·K) at 20 °C
Typical for Austenitic Stainless Steel
Thermal conductivity
λ11 - 21 W/(m·K) at 20 °C
Typical for Austenitic Stainless Steel
Electrical resistivity
ρel8.5E-7 Ω·m at 20 °C
Typical for Austenitic Stainless Steel
Element
Weight %
Comment
16 - 18 %
10 - 14 %
2 %
2 - 3 %
1 %
This material data has been provided by ASTM.