ASTM A213 Grade T12 Heat-Treated

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for Molybdenum Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for Molybdenum Steel

Elongation A50

23.0 °C

30 %

Show Material materials with Elongation A50 of 30 %

Hardness, Brinell

23.0 °C

163 [-]

Show Material materials with Hardness, Brinell of 163 [-]

Hardness, Rockwell B

23.0 °C

85 [-]

Show Material materials with Hardness, Rockwell B of 85 [-]

Hardness, Vickers

23.0 °C

170 [-]

Show Material materials with Hardness, Vickers of 170 [-]

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Molybdenum Steel

Tensile strength

23.0 °C

415 MPa

Show Material materials with Tensile strength of 415 MPa

Yield strength

23.0 °C

220 MPa

Show Material materials with Yield strength of 220 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.29E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.29E-5 1/K

Typical for Molybdenum Steel

Melting point

1382 - 1529 °C

Show Material materials with Melting point of 1382 - 1529 °C

Typical for Molybdenum Steel

Specific heat capacity

23.0 °C

456 J/(kg·K)

Show Material materials with Specific heat capacity of 456 J/(kg·K)

Typical for Molybdenum Steel

Thermal conductivity

23.0 °C

37 - 48 W/(m·K)

Show Material materials with Thermal conductivity of 37 - 48 W/(m·K)

Typical for Molybdenum Steel

Chemical properties

PropertyValue

Carbon

0.05 - 0.15 %

Show Material materials with Carbon of 0.05 - 0.15 %

Chromium

0.8 - 1.25 %

Show Material materials with Chromium of 0.8 - 1.25 %

Manganese

0.3 - 0.61 %

Show Material materials with Manganese of 0.3 - 0.61 %

Molybdenum

0.44 - 0.65 %

Show Material materials with Molybdenum of 0.44 - 0.65 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.5 %

Show Material materials with Silicon of 0.5 %

Sulfur

0.025 %

Show Material materials with Sulfur of 0.025 %