Mechanical

PropertyTemperatureValue

Elongation A200

20.0 °C

18 %

Show Material materials with Elongation A200 of 18 %

Elongation A50

20.0 °C

22 %

Show Material materials with Elongation A50 of 22 %

Tensile strength

20.0 °C

380 - 550 MPa

Show Material materials with Tensile strength of 380 - 550 MPa

Yield strength

20.0 °C

230 MPa

Show Material materials with Yield strength of 230 MPa

Chemical properties

PropertyValue

Carbon

0.05 - 0.21 %

Show Material materials with Carbon of 0.05 - 0.21 %

Chromium

0.5 - 0.8 %

Show Material materials with Chromium of 0.5 - 0.8 %

Manganese

0.55 - 0.8 %

Show Material materials with Manganese of 0.55 - 0.8 %

Molybdenum

0.45 - 0.6 %

Show Material materials with Molybdenum of 0.45 - 0.6 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.15 - 0.4 %

Show Material materials with Silicon of 0.15 - 0.4 %

Sulfur

0.025 %

Show Material materials with Sulfur of 0.025 %