ASTM A53 Grade B Type S

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Properties

General

Density ρ

7.8 - 7.9 g/cm³ at 20 °C

Typical for Medium Carbon Steel

Mechanical

Elastic modulus E

200 - 215 GPa at 20 °C

Typical for Medium Carbon Steel

Poisson's ratio ν

0.29 [-] at 20 °C

Typical for Medium Carbon Steel

Shear modulus G

75 - 80 GPa at 20 °C

Typical for Carbon Steel

Tensile strength Rm

415 MPa at 20 °C

Yield Strength Rp0.2, short transverse Rp0.2,shorttrans_

240 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.32E-5 1/K at 20 °C

Typical for Medium Carbon Steel

Max service temperature Tmax

500 °C

Typical for Carbon Steel

Melting point Tm

1380 - 1514 °C

Typical for Medium Carbon Steel

Electrical

Electrical resistivity ρel

1.43E-7 - 1.74E-7 Ω·m at 20 °C

Typical for Carbon Steel

Chemical properties

Element

Weight %

Comment

Mn

1.2 %

Cr

0.4 %

Cu

0.4 %

Ni

0.4 %

C

0.3 %

More

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.