ASTM A53 Grade A Type S

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperatureComment

Density

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³ at 23.0 °C

23.0 °C

Typical for Low Carbon Steel

Mechanical

PropertyValueTemperatureComment

Elastic modulus

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa at 23.0 °C

23.0 °C

Typical for Low Carbon Steel

Poisson's ratio

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-] at 23.0 °C

23.0 °C

Typical for Low Carbon Steel

Shear modulus

82 GPa

Show Material materials with Shear modulus of 82 GPa at 23.0 °C

23.0 °C

Typical for Low Carbon Steel

Tensile strength

330 MPa

Show Material materials with Tensile strength of 330 MPa at 23.0 °C

23.0 °C

Yield strength Rp0.2

205 MPa

Show Material materials with Yield strength Rp0.2 of 205 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperatureComment

Coefficient of thermal expansion

1.32E-5 - 1.38E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K at 23.0 °C

23.0 °C

Typical for Low Carbon Steel

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Melting point

1480 - 1526 °C

Show Material materials with Melting point of 1480 - 1526 °C

Typical for Low Carbon Steel

Specific heat capacity

465 J/(kg·K)

Show Material materials with Specific heat capacity of 465 J/(kg·K) at 23.0 °C

23.0 °C

Typical for Low Carbon Steel

Thermal conductivity

25 - 93 W/(m·K)

Show Material materials with Thermal conductivity of 25 - 93 W/(m·K) at 23.0 °C

23.0 °C

Typical for Low Carbon Steel

Electrical

PropertyValueTemperatureComment

Electrical resistivity

1.43E-7 - 1.74E-7 Ω·m

Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m at 23.0 °C

23.0 °C

Typical for Carbon Steel

Magnetic

PropertyValueComment

Curie temperature

770 °C

Show Material materials with Curie temperature of 770 °C

Typical for Low Carbon Steel

Chemical properties

Property

Carbon

0.25 %

Chromium

0.4 %

Copper

0.4 %

Manganese

0.95 %

Molybdenum

0.15 %

Nickel

0.4 %

Phosphorus

0.05 %

Sulfur

0.045 %

Vanadium

0.08 %