Maraging 250 Aged

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where Maraging 250 Aged falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

8.2 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

190 GPa at 23 °C

Show Maraging Steel materials with Elastic modulus of 190 GPa at 23 °C

Elongation

A

10 % at 23 °C

Show Maraging Steel materials with Elongation of 10 % at 23 °C

Poisson's ratio

ν

0.3 [-] at 23 °C

Show Maraging Steel materials with Poisson's ratio of 0.3 [-] at 23 °C

Typical for Maraging Steel

Tensile strength

Rm

1800 MPa at 23 °C

Show Maraging Steel materials with Tensile strength of 1800 MPa at 23 °C

Yield strength

YS

1820 MPa at 23 °C

Show Maraging Steel materials with Yield strength of 1820 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.3E-5 1/K at 23 °C

Melting point

Tm

1425 - 1505 °C

Typical for Maraging Steel

Specific heat capacity

cp

440 J/(kg·K) at 23 °C

Thermal conductivity

λ

20 - 25 W/(m·K) at 23 °C

Typical for Maraging Steel

Chemical properties

Element

Weight %

Comment

Fe

66.3 - 71.1 %

Ni

17 - 19 %

Co

7 - 8.5 %

Mo

4.6 - 5.2 %

Ti

0.3 - 0.5 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.