Aged 300 Maraging Steel

.XLSX
.PDF
Save

Properties

General

Density ρ

8.2 g/cm³ at 20 °C

Mechanical

Elastic modulus E

190 GPa at 20 °C

Elongation A

9 % at 20 °C

Tensile strength Rm

2030 MPa at 20 °C

Yield strength YS

2100 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.3E-5 1/K at 20 °C

Specific heat capacity cp

440 J/(kg·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

65 - 68.4 %

Ni

18 - 19 %

Co

8.5 - 9.5 %

Mo

4.6 - 5.2 %

Ti

0.5 - 0.8 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.