Density
ρ8.2 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.3E-5 1/K at 23 °C
Melting point
Tm1425 - 1505 °C
Typical for Maraging Steel
Specific heat capacity
cp440 J/(kg·K) at 23 °C
Thermal conductivity
λ20 - 25 W/(m·K) at 23 °C
Typical for Maraging Steel
Element
Weight %
Comment
65 - 68.4 %
18 - 19 %
8.5 - 9.5 %
4.6 - 5.2 %
0.5 - 0.8 %