General
Property | Value | Temperature |
---|---|---|
Density | 8.2 g/cm³ Show Material materials with Density of 8.2 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 180 GPa Show Material materials with Elastic modulus of 180 GPa at 23.0 °C | 23.0 °C | |
Elongation | 18 % Show Material materials with Elongation of 18 % at 23.0 °C | 23.0 °C | |
Poisson's ratio | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] at 23.0 °C | 23.0 °C | Typical for Maraging Steel |
Tensile strength | 970 MPa Show Material materials with Tensile strength of 970 MPa at 23.0 °C | 23.0 °C | |
Yield strength | 690 MPa Show Material materials with Yield strength of 690 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K at 23.0 °C | 23.0 °C | |
Melting point | 1425 - 1505 °C Show Material materials with Melting point of 1425 - 1505 °C | Typical for Maraging Steel | |
Specific heat capacity | 440 J/(kg·K) Show Material materials with Specific heat capacity of 440 J/(kg·K) at 23.0 °C | 23.0 °C | |
Thermal conductivity | 20 - 25 W/(m·K) Show Material materials with Thermal conductivity of 20 - 25 W/(m·K) at 23.0 °C | 23.0 °C | Typical for Maraging Steel |
Chemical properties
Property | ||
---|---|---|
Aluminium | 0.05 - 0.15 % | |
Boron | 0 - 3E-3 % | |
Calcium | 0 - 0.05 % | |
Carbon | 0 - 0.03 % | |
Cobalt | 8 - 9 % | |
Iron | 67.8 - 71.8 % | |
Manganese | 0 - 0.1 % | |
Molybdenum | 3 - 3.5 % | |
Nickel | 17 - 19 % | |
Phosphorus | 0 - 0.01 % | |
Silicon | 0 - 0.1 % | |
Sulfur | 0 - 0.01 % | |
Titanium | 0.15 - 0.25 % | |
Zirconium | 0 - 0.02 % |