General

Density ρ

7.6 g/cm³ at 20 °C

Mechanical

Elastic modulus E

220 GPa at 20 °C

Elongation A

46 % at 20 °C

Poisson's ratio ν

0.3 [-] at 20 °C

Typical for Austenitic Stainless Steel

Tensile strength Rm

810 MPa at 20 °C

Yield strength YS

460 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.4E-5 1/K at 20 °C

Melting point Tm

1375 - 1450 °C

Typical for Austenitic Stainless Steel

Specific heat capacity cp

460 J/(kg·K) at 20 °C

Thermal conductivity λ

11 - 21 W/(m·K) at 20 °C

Typical for Austenitic Stainless Steel

Electrical

Electrical resistivity ρel

8.5E-7 Ω·m at 20 °C

Typical for Austenitic Stainless Steel

Chemical properties

Element

Weight %

Comment

Fe

62.6 - 68.1 %

Cr

16.5 - 18.5 %

Mn

14 - 15.5 %

Ni

1 - 1.7 %

N

0.32 - 0.4 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.