See where AISI 301LN Annealed falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ7.8 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.2E-5 1/K at 23 °C
Melting point
Tm1230 - 1480 °C
Typical for Austenitic Stainless Steel
Specific heat capacity
cp500 J/(kg·K) at 23 °C
Thermal conductivity
λ15 W/(m·K) at 23 °C
Electrical resistivity
ρel8.5E-7 Ω·m at 23 °C
Typical for Austenitic Stainless Steel
Element
Weight %
Comment
70.2 - 77.9 %
16 - 18.5 %
6 - 8 %
0.07 - 0.2 %
0 - 0.03 %
This material data has been provided by MakeItFrom.com.