Density
ρ7.7 g/cm³ at 23 °C
Coefficient of thermal expansion
α1E-5 1/K at 23 °C
Melting point
Tm1370 °C
Specific heat capacity
cp460 J/(kg·K) at 23 °C
Thermal conductivity
λ30 W/(m·K) at 23 °C
Electrical resistivity
ρel6E-7 Ω·m at 23 °C
Typical for Martensitic Stainless Steel
Element
Weight %
Comment
78.4 - 85 %
14 - 18 %
0.6 - 0.75 %
0 - 1 %
0 - 0.8 %