See where AISI 440B Annealed falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ7.7 g/cm³ at 20 °C
Coefficient of thermal expansion
α1E-5 1/K at 20 °C
Melting point
Tm1370 °C
Specific heat capacity
cp430 J/(kg·K) at 20 °C
Thermal conductivity
λ15 W/(m·K) at 20 °C
Electrical resistivity
ρel6E-7 Ω·m at 20 °C
Typical for Martensitic Stainless Steel
Element
Weight %
Comment
76.6 - 83.3 %
16 - 19 %
0.75 - 1 %
0.07 - 0.12 %
0 - 1 %
This material data has been provided by MakeItFrom.com.