AISI 1095 Annealed And Cold Drawn

View suppliers (18)
Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

210 GPa

Show Material materials with Elastic modulus of 210 GPa

Elongation

23.0 °C

10 %

Show Material materials with Elongation of 10 %

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for High Carbon Steel

Shear modulus

23.0 °C

81 GPa

Show Material materials with Shear modulus of 81 GPa

Typical for High Carbon Steel

Tensile strength

23.0 °C

680 MPa

Show Material materials with Tensile strength of 680 MPa

Yield strength

23.0 °C

530 MPa

Show Material materials with Yield strength of 530 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Melting point

1289 - 1478 °C

Show Material materials with Melting point of 1289 - 1478 °C

Typical for High Carbon Steel

Specific heat capacity

23.0 °C

450 J/(kg·K)

Show Material materials with Specific heat capacity of 450 J/(kg·K)

Thermal conductivity

23.0 °C

36 W/(m·K)

Show Material materials with Thermal conductivity of 36 W/(m·K)

Typical for High Carbon Steel

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

1.43E-7 - 1.74E-7 Ω·m

Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m

Typical for Carbon Steel

Chemical properties

PropertyValue

Carbon

0.9 - 1 %

Show Material materials with Carbon of 0.9 - 1 %

Iron

98.4 - 98.8 %

Show Material materials with Iron of 98.4 - 98.8 %

Manganese

0.3 - 0.5 %

Show Material materials with Manganese of 0.3 - 0.5 %

Phosphorus

0 - 0.04 %

Show Material materials with Phosphorus of 0 - 0.04 %

Sulfur

0 - 0.05 %

Show Material materials with Sulfur of 0 - 0.05 %