UNS S30600 Annealed

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where UNS S30600 Annealed falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

7.7 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

200 GPa at 23 °C

Show Austenitic Stainless Steel materials with Elastic modulus of 200 GPa at 23 °C

Elongation

A

46 % at 23 °C

Show Austenitic Stainless Steel materials with Elongation of 46 % at 23 °C

Poisson's ratio

ν

0.3 [-] at 23 °C

Show Austenitic Stainless Steel materials with Poisson's ratio of 0.3 [-] at 23 °C

Typical for Austenitic Stainless Steel

Shear modulus

G

77 GPa at 23 °C

Show Austenitic Stainless Steel materials with Shear modulus of 77 GPa at 23 °C

Typical for Austenitic Stainless Steel

Tensile strength

Rm

620 MPa at 23 °C

Show Austenitic Stainless Steel materials with Tensile strength of 620 MPa at 23 °C

Yield strength

YS

280 MPa at 23 °C

Show Austenitic Stainless Steel materials with Yield strength of 280 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.2E-5 1/K at 23 °C

Melting point

Tm

1230 - 1480 °C

Typical for Austenitic Stainless Steel

Specific heat capacity

cp

460 J/(kg·K) at 23 °C

Thermal conductivity

λ

14 W/(m·K) at 23 °C

Electrical

Electrical resistivity

ρel

8.5E-7 Ω·m at 23 °C

Typical for Austenitic Stainless Steel

Chemical properties

Element

Weight %

Comment

Fe

58.7 - 65.8 %

Cr

16.5 - 18.5 %

Ni

14 - 16 %

Si

3.7 - 4.5 %

C

0 - 0.018 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.