See where UNS S32550 Annealed falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ7.8 g/cm³ at 20 °C
Coefficient of thermal expansion
α1.3E-5 1/K at 20 °C
Max service temperature
Tmax300 °C
Typical for Duplex Stainless Steel
Melting point
Tm1375 - 1450 °C
Typical for Duplex Stainless Steel
Specific heat capacity
cp500 J/(kg·K) at 20 °C
Thermal conductivity
λ15 W/(m·K) at 20 °C
Element
Weight %
Comment
56.4 - 67 %
24 - 27 %
4.5 - 8 %
2.9 - 4 %
1 - 2.5 %
This material data has been provided by MakeItFrom.com.