See where AISI 1547 Cold Drawn falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ7.8 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.2E-5 1/K at 23 °C
Max service temperature
Tmax500 °C
Typical for Carbon Steel
Melting point
Tm1380 - 1514 °C
Typical for Medium Carbon Steel
Specific heat capacity
cp450 J/(kg·K) at 23 °C
Thermal conductivity
λ21 - 52 W/(m·K) at 23 °C
Typical for Medium Carbon Steel
Electrical resistivity
ρel1.43E-7 - 1.74E-7 Ω·m at 23 °C
Typical for Carbon Steel
Element
Weight %
Comment
97.8 - 98.2 %
1.4 - 1.7 %
0.43 - 0.51 %
0 - 0.04 %
0 - 0.05 %