General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 7.6 g/cm³ Show Material materials with Density of 7.6 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 220 GPa Show Material materials with Elastic modulus of 220 GPa | |
Elongation | 23.0 °C | 12 % Show Material materials with Elongation of 12 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Austenitic Stainless Steel |
Shear modulus | 23.0 °C | 77 GPa Show Material materials with Shear modulus of 77 GPa | Typical for Austenitic Stainless Steel |
Tensile strength | 23.0 °C | 1470 MPa Show Material materials with Tensile strength of 1470 MPa | |
Yield strength | 23.0 °C | 1110 MPa Show Material materials with Yield strength of 1110 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.4E-5 1/K | |
Melting point | 1230 - 1480 °C Show Material materials with Melting point of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Specific heat capacity | 23.0 °C | 460 J/(kg·K) Show Material materials with Specific heat capacity of 460 J/(kg·K) | |
Thermal conductivity | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Thermal conductivity of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Electrical resistivity of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.12 - 0.25 % Show Material materials with Carbon of 0.12 - 0.25 % |
Chromium | 16.5 - 18.5 % Show Material materials with Chromium of 16.5 - 18.5 % |
Iron | 62.6 - 68.1 % Show Material materials with Iron of 62.6 - 68.1 % |
Manganese | 14 - 15.5 % Show Material materials with Manganese of 14 - 15.5 % |
Nickel | 1 - 1.7 % Show Material materials with Nickel of 1 - 1.7 % |
Nitrogen | 0.32 - 0.4 % Show Material materials with Nitrogen of 0.32 - 0.4 % |
Phosphorus | 0 - 0.06 % Show Material materials with Phosphorus of 0 - 0.06 % |
Silicon | 0 - 1 % Show Material materials with Silicon of 0 - 1 % |
Sulfur | 0 - 0.03 % Show Material materials with Sulfur of 0 - 0.03 % |