General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 7.9 g/cm³ Show Material materials with Density of 7.9 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 GPa Show Material materials with Elastic modulus of 200 GPa | |
Elongation | 23.0 °C | 9.2 % Show Material materials with Elongation of 9.2 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Austenitic Stainless Steel |
Shear modulus | 23.0 °C | 77 GPa Show Material materials with Shear modulus of 77 GPa | Typical for Austenitic Stainless Steel |
Tensile strength | 23.0 °C | 1190 MPa Show Material materials with Tensile strength of 1190 MPa | |
Yield strength | 23.0 °C | 870 MPa Show Material materials with Yield strength of 870 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 1/K |
Melting point | 1380 °C Show Material materials with Melting point of 1380 °C | |
Specific heat capacity | 23.0 °C | 490 J/(kg·K) Show Material materials with Specific heat capacity of 490 J/(kg·K) |
Thermal conductivity | 23.0 °C | 15 W/(m·K) Show Material materials with Thermal conductivity of 15 W/(m·K) |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Electrical resistivity of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0 - 0.03 % Show Material materials with Carbon of 0 - 0.03 % |
Chromium | 16 - 19 % Show Material materials with Chromium of 16 - 19 % |
Iron | 59.8 - 72 % Show Material materials with Iron of 59.8 - 72 % |
Manganese | 0 - 2 % Show Material materials with Manganese of 0 - 2 % |
Molybdenum | 2 - 3 % Show Material materials with Molybdenum of 2 - 3 % |
Nickel | 10 - 15 % Show Material materials with Nickel of 10 - 15 % |
Nitrogen | 0 - 0.1 % Show Material materials with Nitrogen of 0 - 0.1 % |
Phosphorus | 0 - 0.05 % Show Material materials with Phosphorus of 0 - 0.05 % |
Silicon | 0 - 1 % Show Material materials with Silicon of 0 - 1 % |
Sulfur | 0 - 0.03 % Show Material materials with Sulfur of 0 - 0.03 % |