AISI 420 Hardened

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperature

Density

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³ at 23.0 °C

23.0 °C

Mechanical

PropertyValueTemperatureComment

Elastic modulus

210 GPa

Show Material materials with Elastic modulus of 210 GPa at 23.0 °C

23.0 °C

Elongation

12 %

Show Material materials with Elongation of 12 % at 23.0 °C

23.0 °C

Poisson's ratio

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-] at 23.0 °C

23.0 °C

Typical for Martensitic Stainless Steel

Shear modulus

77 GPa

Show Material materials with Shear modulus of 77 GPa at 23.0 °C

23.0 °C

Typical for Martensitic Stainless Steel

Tensile strength

980 MPa

Show Material materials with Tensile strength of 980 MPa at 23.0 °C

23.0 °C

Yield strength

760 MPa

Show Material materials with Yield strength of 760 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperature

Coefficient of thermal expansion

1E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1E-5 1/K at 23.0 °C

23.0 °C

Melting point

1450 °C

Show Material materials with Melting point of 1450 °C

Specific heat capacity

460 J/(kg·K)

Show Material materials with Specific heat capacity of 460 J/(kg·K) at 23.0 °C

23.0 °C

Thermal conductivity

30 W/(m·K)

Show Material materials with Thermal conductivity of 30 W/(m·K) at 23.0 °C

23.0 °C

Electrical

PropertyValueTemperatureComment

Electrical resistivity

6E-7 Ω·m

Show Material materials with Electrical resistivity of 6E-7 Ω·m at 23.0 °C

23.0 °C

Typical for Martensitic Stainless Steel

Chemical properties

Property

Carbon

0.15 - 0.4 %

Chromium

12 - 14 %

Iron

82.3 - 87.9 %

Manganese

0 - 1.5 %

Molybdenum

0 - 0.5 %

Nickel

0 - 0.75 %

Phosphorus

0 - 0.04 %

Silicon

0 - 1 %

Sulfur

0 - 0.03 %