General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 7.7 g/cm³ Show Material materials with Density of 7.7 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 210 GPa Show Material materials with Elastic modulus of 210 GPa | |
Elongation | 23.0 °C | 3 % Show Material materials with Elongation of 3 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Martensitic Stainless Steel |
Shear modulus | 23.0 °C | 77 GPa Show Material materials with Shear modulus of 77 GPa | Typical for Martensitic Stainless Steel |
Tensile strength | 23.0 °C | 1930 MPa Show Material materials with Tensile strength of 1930 MPa | |
Yield strength | 23.0 °C | 1860 MPa Show Material materials with Yield strength of 1860 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1E-5 1/K |
Melting point | 1370 °C Show Material materials with Melting point of 1370 °C | |
Specific heat capacity | 23.0 °C | 430 J/(kg·K) Show Material materials with Specific heat capacity of 430 J/(kg·K) |
Thermal conductivity | 23.0 °C | 15 W/(m·K) Show Material materials with Thermal conductivity of 15 W/(m·K) |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | 6E-7 Ω·m Show Material materials with Electrical resistivity of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.75 - 1 % Show Material materials with Carbon of 0.75 - 1 % |
Chromium | 16 - 19 % Show Material materials with Chromium of 16 - 19 % |
Iron | 76.6 - 83.3 % Show Material materials with Iron of 76.6 - 83.3 % |
Manganese | 0 - 1 % Show Material materials with Manganese of 0 - 1 % |
Molybdenum | 0 - 1.3 % Show Material materials with Molybdenum of 0 - 1.3 % |
Phosphorus | 0 - 0.04 % Show Material materials with Phosphorus of 0 - 0.04 % |
Silicon | 0 - 1 % Show Material materials with Silicon of 0 - 1 % |
Sulfur | 0 - 0.015 % Show Material materials with Sulfur of 0 - 0.015 % |
Vanadium | 0.07 - 0.12 % Show Material materials with Vanadium of 0.07 - 0.12 % |