AISI 422 Heat Treated

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where AISI 422 Heat Treated falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

7.9 g/cm³ at 20 °C

Mechanical

Elastic modulus

E

200 GPa at 20 °C

Elongation

A

15 % at 20 °C

Poisson's ratio

ν

0.3 [-] at 20 °C

Typical for Martensitic Stainless Steel

Shear modulus

G

77 GPa at 20 °C

Typical for Martensitic Stainless Steel

Tensile strength

Rm

1110 MPa at 20 °C

Yield strength

YS

870 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

1.2E-5 1/K at 20 °C

Melting point

Tm

1470 °C

Specific heat capacity

cp

460 J/(kg·K) at 20 °C

Thermal conductivity

λ

24 W/(m·K) at 20 °C

Electrical

Electrical resistivity

ρel

6E-7 Ω·m at 20 °C

Typical for Martensitic Stainless Steel

Chemical properties

Element

Weight %

Comment

Fe

81.9 - 85.8 %

Cr

11 - 12.5 %

Mo

0.9 - 1.3 %

W

0.9 - 1.3 %

Mn

0.5 - 1 %

More

This material data has been provided by MakeItFrom.com.