AISI 1086 Hot Rolled

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where AISI 1086 Hot Rolled falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

7.8 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

210 GPa at 23 °C

Show High Carbon Steel materials with Elastic modulus of 210 GPa at 23 °C

Elongation

A

12 % at 23 °C

Show High Carbon Steel materials with Elongation of 12 % at 23 °C

Poisson's ratio

ν

0.29 [-] at 23 °C

Show High Carbon Steel materials with Poisson's ratio of 0.29 [-] at 23 °C

Typical for High Carbon Steel

Shear modulus

G

81 GPa at 23 °C

Show High Carbon Steel materials with Shear modulus of 81 GPa at 23 °C

Typical for High Carbon Steel

Tensile strength

Rm

890 MPa at 23 °C

Show High Carbon Steel materials with Tensile strength of 890 MPa at 23 °C

Yield strength

YS

490 MPa at 23 °C

Show High Carbon Steel materials with Yield strength of 490 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.2E-5 1/K at 23 °C

Max service temperature

Tmax

500 °C

Typical for Carbon Steel

Melting point

Tm

1289 - 1478 °C

Typical for High Carbon Steel

Specific heat capacity

cp

450 J/(kg·K) at 23 °C

Thermal conductivity

λ

36 W/(m·K) at 23 °C

Typical for High Carbon Steel

Electrical

Electrical resistivity

ρel

1.43E-7 - 1.74E-7 Ω·m at 23 °C

Typical for Carbon Steel

Chemical properties

Element

Weight %

Comment

Fe

98.5 - 98.9 %

C

0.8 - 0.93 %

Mn

0.3 - 0.5 %

P

0 - 0.04 %

S

0 - 0.05 %

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.