AISI 1527 Hot Rolled

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where AISI 1527 Hot Rolled falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

7.8 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

210 GPa at 23 °C

Show Manganese Steel materials with Elastic modulus of 210 GPa at 23 °C

Elongation

A

21 % at 23 °C

Show Manganese Steel materials with Elongation of 21 % at 23 °C

Poisson's ratio

ν

0.29 [-] at 23 °C

Show Manganese Steel materials with Poisson's ratio of 0.29 [-] at 23 °C

Typical for Manganese Steel

Tensile strength

Rm

600 MPa at 23 °C

Show Manganese Steel materials with Tensile strength of 600 MPa at 23 °C

Yield strength

YS

330 MPa at 23 °C

Show Manganese Steel materials with Yield strength of 330 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.2E-5 1/K at 23 °C

Melting point

Tm

1382 - 1529 °C

Typical for Manganese Steel

Specific heat capacity

cp

450 J/(kg·K) at 23 °C

Thermal conductivity

λ

14 - 16 W/(m·K) at 23 °C

Typical for Manganese Steel

Chemical properties

Element

Weight %

Comment

Fe

98.1 - 98.6 %

Mn

1.2 - 1.5 %

C

0.22 - 0.29 %

P

0 - 0.04 %

S

0 - 0.05 %

This material data has been provided by MakeItFrom.com.