Wrought Copper Bronze Aluminium Bronze
AMPCO® 45 Extruded and drawn rodsSuministrada por:
AMPCO METALCast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95300 Heat-TreatedSuministrada por:
1 proveedor Matmatch
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95300 HT, Heat-TreatedSuministrada por:
1 proveedor Matmatch
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95500 Heat-TreatedSuministrada por:
1 proveedor Matmatch
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95500 HT, Heat-TreatedSuministrada por:
1 proveedor Matmatch