ASTM A564 Grade S13800 Precipitation hardened

Want to keep this datasheet? Save it now in your required format

Description

AMS5629 13/8PH is a martensitic precipitation hardening stainless steel. Heat treatment provides 13/8PH with high strength. It comes in various conditions offering an array of properties. It offers excellent weldability, corrosion resistance and machinability.

Related Standards

Equivalent Materials

This material data has been provided by Righton Blackburns,Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.75 g/cm³

Show Material materials with Density of 7.75 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

196 GPa

Show Material materials with Elastic modulus of 196 GPa

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.08E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.08E-5 1/K

Thermal conductivity

23.0 °C

18.4 W/(m·K)

Show Material materials with Thermal conductivity of 18.4 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

8E-8 Ω·m

Show Material materials with Electrical resistivity of 8E-8 Ω·m

Chemical properties

PropertyValue

Aluminium

0.9 - 1.35 %

Show Material materials with Aluminium of 0.9 - 1.35 %

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Chromium

12.25 - 13.25 %

Show Material materials with Chromium of 12.25 - 13.25 %

Iron

Balance

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

Molybdenum

2 - 2.5 %

Show Material materials with Molybdenum of 2 - 2.5 %

Nickel

7.5 - 8.5 %

Show Material materials with Nickel of 7.5 - 8.5 %

Nitrogen

0.01 %

Show Material materials with Nitrogen of 0.01 %

Phosphorus

0.01 %

Show Material materials with Phosphorus of 0.01 %

Silicon

0.1 %

Show Material materials with Silicon of 0.1 %

Sulfur

0.01 %

Show Material materials with Sulfur of 0.01 %

Technological properties

Property
Application areas

Landing Gear, Valves, Shafts, Petrochemical Components