General Polyethylene, low density (PE-LD)

Alternative and trade names
Lupolen®, Purell®, Pharmalene®, Riblene®
.XLSX
.PDF
Save

Description

Unfilled, no additives.

Properties

Electrical

Dielectric constant εr

2.2 - 2.3 [-] at 20 °C

Electrical resistivity ρel

1.00E+15 Ω·m at 20 °C

General

Density ρ

0.92 g/cm³ at 20 °C

Mechanical

Elastic modulus E

0.2 - 0.4 GPa at 20 °C

Elongation A

100 - 1000 % at 20 °C

Impact strength, Charpy unnotched Iunnot

no break

Max allowed stress σmax

6 - 17 MPa at 20 °C

at 15-25% strain

Optical

Transparency

no

Thermal

Coefficient of thermal expansion α

2.3E-4 - 2.5E-4 1/K at 20 °C

Flammability

UL 94 HB

Max service temperature, long Tmaxlong

60 - 75 °C

Max service temperature, short Tmaxshort

80 - 90 °C

Melting point Tm

105 - 120 °C

Specific heat capacity cp

2100 - 2500 J/(kg·K) at 20 °C

Thermal conductivity λ

0.32 - 0.4 W/(m·K) at 20 °C

Technological properties

Application areas

Films for packaging, agricultural films, carrying bags, heavy-duty sacks, wine bottle closures

Processing methods

Injection molding, blow molding, extrusion, compression molding, thermoforming, coating

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.