SAE J217 Grade 17-7PH

Want to keep this datasheet? Save it now in your required format

Description

Grade J217 is a high-quality corrosion-resisting steel wire, cold drawn, formed, and heat treated to produce uniform mechanical properties. It is magnetic in all conditions. It is intended for the manufacture of springs and wire forms that are to be heat treated after forming to enhance the spring properties.

Related Standards

Equivalent Materials

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Typical for Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Chemical properties

PropertyValueComment

Aluminium

0.75 - 1.5 %

Show Material materials with Aluminium of 0.75 - 1.5 %

Carbon

0.09 %

Show Material materials with Carbon of 0.09 %

Chromium

16 - 18 %

Show Material materials with Chromium of 16 - 18 %

Iron

70.58 - 76.75 %

Show Material materials with Iron of 70.58 - 76.75 %

balance

Manganese

1 %

Show Material materials with Manganese of 1 %

Nickel

6.5 - 7.75 %

Show Material materials with Nickel of 6.5 - 7.75 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %