General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 1.17 % Show Material materials with Aluminium of 1.17 % |
Carbon | 0.07 % Show Material materials with Carbon of 0.07 % |
Chromium | 17 % Show Material materials with Chromium of 17 % |
Iron | 70.58 - 76.75 % Show Material materials with Iron of 70.58 - 76.75 % |
Manganese | 0.5 % Show Material materials with Manganese of 0.5 % |
Nickel | 7.1 % Show Material materials with Nickel of 7.1 % |
Silicon | 0.3 % Show Material materials with Silicon of 0.3 % |