General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.2 % Show Material materials with Aluminium of 0.2 % |
Boron | 4E-3 % Show Material materials with Boron of 4E-3 % |
Carbon | 0.05 % Show Material materials with Carbon of 0.05 % |
Chromium | 15 % Show Material materials with Chromium of 15 % |
Iron | 49.14 - 59.5 % Show Material materials with Iron of 49.14 - 59.5 % |
Manganese | 1.4 % Show Material materials with Manganese of 1.4 % |
Molybdenum | 1.3 % Show Material materials with Molybdenum of 1.3 % |
Nickel | 26 % Show Material materials with Nickel of 26 % |
Silicon | 0.4 % Show Material materials with Silicon of 0.4 % |
Titanium | 2.15 % Show Material materials with Titanium of 2.15 % |
Vanadium | 0.3 % Show Material materials with Vanadium of 0.3 % |