Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 5 % Show Material materials with Aluminium of 5 % |
Boron | 0.015 % Show Material materials with Boron of 0.015 % |
Carbon | 0.15 % Show Material materials with Carbon of 0.15 % |
Chromium | 9 % Show Material materials with Chromium of 9 % |
Cobalt | 10 % Show Material materials with Cobalt of 10 % |
Iron | 60.28 - 100 % Show Material materials with Iron of 60.28 - 100 % |
Niobium | 1 % Show Material materials with Niobium of 1 % |
Titanium | 2 % Show Material materials with Titanium of 2 % |
Tungsten | 12.5 % Show Material materials with Tungsten of 12.5 % |
Zirconium | 0.05 % Show Material materials with Zirconium of 0.05 % |