General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 200 GPa Show Material materials with Elastic modulus of 200 GPa | |
100.0 °C | 195 GPa Show Material materials with Elastic modulus of 195 GPa | ||
200.0 °C | 185 GPa Show Material materials with Elastic modulus of 185 GPa | ||
300.0 °C | 175 GPa Show Material materials with Elastic modulus of 175 GPa | ||
400.0 °C | 170 GPa Show Material materials with Elastic modulus of 170 GPa | ||
Elongation | 20.0 °C | 10 % Show Material materials with Elongation of 10 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Tensile strength | 20.0 °C | 1000 - 1200 MPa Show Material materials with Tensile strength of 1000 - 1200 MPa | |
Yield strength Rp0.2 | 20.0 °C | 860 MPa Show Material materials with Yield strength Rp0.2 of 860 MPa | |
100.0 °C | 785 MPa Show Material materials with Yield strength Rp0.2 of 785 MPa | ||
150.0 °C | 755 MPa Show Material materials with Yield strength Rp0.2 of 755 MPa | ||
200.0 °C | 730 MPa Show Material materials with Yield strength Rp0.2 of 730 MPa | ||
250.0 °C | 710 MPa Show Material materials with Yield strength Rp0.2 of 710 MPa | ||
300.0 °C | 690 MPa Show Material materials with Yield strength Rp0.2 of 690 MPa | ||
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.09E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.09E-5 1/K |
300.0 °C | 1.11E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.11E-5 1/K | |
Specific heat capacity | 20.0 °C | 500 J/(kg·K) Show Material materials with Specific heat capacity of 500 J/(kg·K) |
Thermal conductivity | 20.0 °C | 16 W/(m·K) Show Material materials with Thermal conductivity of 16 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 20.0 °C | 7.1E-7 Ω·m Show Material materials with Electrical resistivity of 7.1E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Carbon | 0.07 % Show Material materials with Carbon of 0.07 % |
Chromium | 13 - 15 % Show Material materials with Chromium of 13 - 15 % |
Copper | 1.2 - 2 % Show Material materials with Copper of 1.2 - 2 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Molybdenum | 1.2 - 2 % Show Material materials with Molybdenum of 1.2 - 2 % |
Nickel | 5 - 6 % Show Material materials with Nickel of 5 - 6 % |
Niobium | 0.15 - 0.6 % Show Material materials with Niobium of 0.15 - 0.6 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 0.7 % Show Material materials with Silicon of 0.7 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |