EN 10139 Grade DC05 cold rolled, skin passed

Want to keep this datasheet? Save it now in your required format

Description

Cold rolled uncoated low carbon steel narrow strip for cold forming.,The non-alloy steel DC05 acc. to DIN EN 10130 is as special deep-draw quality suitable for cold forming of complexest profile forms, components and molded parts.To freedom of stretcher strains applies a period of 6 months after provision of the products for surface type A and B. Welding: DC05 is weldable by the following welding methods: MAG (metal-active-gas), plasma welding, laser welding, compression weld welding, resistance welding (spot, roll weld, buckle welding), arc welding. The steel acts as substrate for surface refined and coated bands and sheets. Application of DC05: car manufacturing, construction trade, traffic system. Acc. to DIN EN 10139 DC05 is offered as cold rolled band or bar, cut in strength range HK270.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for Low Carbon Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for Low Carbon Steel

Elongation

20.0 °C

42 %

Show Material materials with Elongation of 42 %

Elongation A50

20.0 °C

34 - 42 %

Show Material materials with Elongation A50 of 34 - 42 %

Elongation A80

20.0 °C

32 - 40 %

Show Material materials with Elongation A80 of 32 - 40 %

Hardness, Vickers

20.0 °C

100 - 110 [-]

Show Material materials with Hardness, Vickers of 100 - 110 [-]

Poisson's ratio

20.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Low Carbon Steel

Tensile strength

20.0 °C

270 - 330 MPa

Show Material materials with Tensile strength of 270 - 330 MPa

Yield strength

20.0 °C

140 - 220 MPa

Show Material materials with Yield strength of 140 - 220 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

1.32E-5 - 1.38E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K

Typical for Low Carbon Steel

Melting point

1480 - 1526 °C

Show Material materials with Melting point of 1480 - 1526 °C

Typical for Low Carbon Steel

Magnetic

PropertyValueComment

Curie temperature

770 °C

Show Material materials with Curie temperature of 770 °C

Typical for Low Carbon Steel

Chemical properties

PropertyValue

Carbon

0.06 %

Show Material materials with Carbon of 0.06 %

Manganese

0.35 %

Show Material materials with Manganese of 0.35 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Sulfur

0.025 %

Show Material materials with Sulfur of 0.025 %