General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.65 - 7.7 g/cm³ Show Material materials with Density of 7.65 - 7.7 g/cm³ |
Mechanical
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | -100.0 °C | 9.2E-6 1/K Show Material materials with Coefficient of thermal expansion of 9.2E-6 1/K |
20.0 °C | 9.9E-6 1/K Show Material materials with Coefficient of thermal expansion of 9.9E-6 1/K | |
100.0 °C | 1.03E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.03E-5 1/K | |
200.0 °C | 1.08E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.08E-5 1/K | |
300.0 °C | 1.12E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.12E-5 1/K | |
400.0 °C | 1.16E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.16E-5 1/K | |
500.0 °C | 1.19E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.19E-5 1/K | |
600.0 °C | 1.21E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.21E-5 1/K | |
700.0 °C | 1.24E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.24E-5 1/K | |
800.0 °C | 1.29E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.29E-5 1/K | |
900.0 °C | 1.34E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.34E-5 1/K | |
1000.0 °C | 1.39E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.39E-5 1/K | |
Specific heat capacity | 20.0 °C | 450 J/(kg·K) Show Material materials with Specific heat capacity of 450 J/(kg·K) |
100.0 °C | 482 J/(kg·K) Show Material materials with Specific heat capacity of 482 J/(kg·K) | |
200.0 °C | 506 J/(kg·K) Show Material materials with Specific heat capacity of 506 J/(kg·K) | |
300.0 °C | 525 J/(kg·K) Show Material materials with Specific heat capacity of 525 J/(kg·K) | |
400.0 °C | 547 J/(kg·K) Show Material materials with Specific heat capacity of 547 J/(kg·K) | |
500.0 °C | 576 J/(kg·K) Show Material materials with Specific heat capacity of 576 J/(kg·K) | |
600.0 °C | 616 J/(kg·K) Show Material materials with Specific heat capacity of 616 J/(kg·K) | |
Thermal conductivity | 20.0 °C | 19.6 W/(m·K) Show Material materials with Thermal conductivity of 19.6 W/(m·K) |
Thermal diffusivity | 20.0 °C | 5.7 mm²/s Show Material materials with Thermal diffusivity of 5.7 mm²/s |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 20.0 °C | 6.17E-7 Ω·m Show Material materials with Electrical resistivity of 6.17E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Carbon | 0.95 - 1.1 % Show Material materials with Carbon of 0.95 - 1.1 % |
Chromium | 16 - 18 % Show Material materials with Chromium of 16 - 18 % |
Copper | 0.3 % Show Material materials with Copper of 0.3 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Molybdenum | 0.35 - 0.75 % Show Material materials with Molybdenum of 0.35 - 0.75 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |