JIS G4307 Grade SUS440A cold-rolled, annealed, quenched and tempered

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

15 %

Show Material materials with Elongation of 15 %

Tensile strength

20.0 °C

588 MPa

Show Material materials with Tensile strength of 588 MPa

Yield strength

20.0 °C

245 MPa

Show Material materials with Yield strength of 245 MPa

Chemical properties

PropertyValue

Carbon

0.6 - 0.75 %

Show Material materials with Carbon of 0.6 - 0.75 %

Chromium

16 - 18 %

Show Material materials with Chromium of 16 - 18 %

Iron

77.83 - 83.4 %

Show Material materials with Iron of 77.83 - 83.4 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Molybdenum

0.75 %

Show Material materials with Molybdenum of 0.75 %

Nickel

0.6 %

Show Material materials with Nickel of 0.6 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Technological properties

Property
Processing history

cold-rolled, annealed, quenched and tempered