Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A5

20.0 °C

5 - 20 %

Show Material materials with Elongation A5 of 5 - 20 %

Hardness, Vickers

20.0 °C

200 - 450 [-]

Show Material materials with Hardness, Vickers of 200 - 450 [-]

Tensile strength

20.0 °C

1030 - 1420 MPa

Show Material materials with Tensile strength of 1030 - 1420 MPa

Chemical properties

PropertyValue

Aluminium

0.75 - 1.5 %

Show Material materials with Aluminium of 0.75 - 1.5 %

Carbon

0.09 %

Show Material materials with Carbon of 0.09 %

Chromium

16 - 18 %

Show Material materials with Chromium of 16 - 18 %

Iron

70.59 - 76.75 %

Show Material materials with Iron of 70.59 - 76.75 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Nickel

6.5 - 7.75 %

Show Material materials with Nickel of 6.5 - 7.75 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Technological properties

Property
Processing history

as cold-rolled, or either as solution-treated or as annealed