Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 20.0 °C | 5 - 6 % Show Material materials with Elongation of 5 - 6 % |
Reduction of area | 20.0 °C | 25 % Show Material materials with Reduction of area of 25 % |
Tensile strength | 20.0 °C | 1240 - 1550 MPa Show Material materials with Tensile strength of 1240 - 1550 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 1100 - 1380 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 1100 - 1380 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.75 - 1.25 % Show Material materials with Aluminium of 0.75 - 1.25 % |
Carbon | 0.09 % Show Material materials with Carbon of 0.09 % |
Chromium | 14 - 15.25 % Show Material materials with Chromium of 14 - 15.25 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Molybdenum | 2 - 2.75 % Show Material materials with Molybdenum of 2 - 2.75 % |
Nickel | 6.5 - 7.75 % Show Material materials with Nickel of 6.5 - 7.75 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.5 % Show Material materials with Silicon of 0.5 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |