General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 10 % Show Material materials with Elongation A50 of 10 % | |
Hardness, Brinell | 23.0 °C | 302 [-] Show Material materials with Hardness, Brinell of 302 [-] | |
Hardness, Rockwell C | 23.0 °C | 32 [-] Show Material materials with Hardness, Rockwell C of 32 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 45 % Show Material materials with Reduction of area of 45 % | |
Tensile strength | 23.0 °C | 825 MPa Show Material materials with Tensile strength of 825 MPa | |
Yield strength | 23.0 °C | 515 MPa Show Material materials with Yield strength of 515 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.4 % Show Material materials with Aluminium of 0.4 % |
Carbon | 0.08 % Show Material materials with Carbon of 0.08 % |
Chromium | 16 - 17.5 % Show Material materials with Chromium of 16 - 17.5 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Nickel | 6 - 7.5 % Show Material materials with Nickel of 6 - 7.5 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |
Titanium | 0.4 - 1.2 % Show Material materials with Titanium of 0.4 - 1.2 % |