General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 14 % Show Material materials with Elongation A50 of 14 % | |
Hardness, Brinell | 23.0 °C | 283 [-] Show Material materials with Hardness, Brinell of 283 [-] | |
Hardness, Rockwell C | 23.0 °C | 30 [-] Show Material materials with Hardness, Rockwell C of 30 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 50 % Show Material materials with Reduction of area of 50 % | |
Tensile strength | 23.0 °C | 930 MPa Show Material materials with Tensile strength of 930 MPa | |
Yield strength | 23.0 °C | 620 MPa Show Material materials with Yield strength of 620 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.9 - 1.35 % Show Material materials with Aluminium of 0.9 - 1.35 % |
Carbon | 0.05 % Show Material materials with Carbon of 0.05 % |
Chromium | 12.25 - 13.25 % Show Material materials with Chromium of 12.25 - 13.25 % |
Manganese | 0.2 % Show Material materials with Manganese of 0.2 % |
Molybdenum | 2 - 2.5 % Show Material materials with Molybdenum of 2 - 2.5 % |
Nickel | 7.5 - 8.5 % Show Material materials with Nickel of 7.5 - 8.5 % |
Phosphorus | 0.01 % Show Material materials with Phosphorus of 0.01 % |
Silicon | 0.1 % Show Material materials with Silicon of 0.1 % |
Sulfur | 8E-3 % Show Material materials with Sulfur of 8E-3 % |