General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 11 - 16 % Show Material materials with Elongation A50 of 11 - 16 % | |
Hardness, Brinell | 23.0 °C | 285 [-] Show Material materials with Hardness, Brinell of 285 [-] | |
Hardness, Rockwell C | 23.0 °C | 30 [-] Show Material materials with Hardness, Rockwell C of 30 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 30 - 50 % Show Material materials with Reduction of area of 30 - 50 % | |
Tensile strength | 23.0 °C | 895 MPa Show Material materials with Tensile strength of 895 MPa | |
Yield strength | 23.0 °C | 725 MPa Show Material materials with Yield strength of 725 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.05 % Show Material materials with Carbon of 0.05 % |
Chromium | 14 - 16 % Show Material materials with Chromium of 14 - 16 % |
Copper | 1.25 - 1.75 % Show Material materials with Copper of 1.25 - 1.75 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Molybdenum | 0.5 - 1 % Show Material materials with Molybdenum of 0.5 - 1 % |
Nickel | 5 - 7 % Show Material materials with Nickel of 5 - 7 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |