General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Hardness, Brinell | 23.0 °C | 255 [-] Show Material materials with Hardness, Brinell of 255 [-] | |
Hardness, Rockwell C | 23.0 °C | 25 [-] Show Material materials with Hardness, Rockwell C of 25 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.95 - 1.2 % Show Material materials with Carbon of 0.95 - 1.2 % |
Chromium | 16 - 18 % Show Material materials with Chromium of 16 - 18 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Molybdenum | 0.4 - 0.8 % Show Material materials with Molybdenum of 0.4 - 0.8 % |
Oxygen | 2E-3 % Show Material materials with Oxygen of 2E-3 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |