Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 8.8 g/cm³ Show Material materials with Density of 8.8 g/cm³ | Typical for Nickel Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Nickel Steel |
Hardness, Rockwell C | 20.0 °C | 60 [-] Show Material materials with Hardness, Rockwell C of 60 [-] | |
Hardness, Vickers | 20.0 °C | 700 [-] Show Material materials with Hardness, Vickers of 700 [-] | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Nickel Steel |
Shear modulus | 23.0 °C | 76 GPa Show Material materials with Shear modulus of 76 GPa | Typical for Nickel Steel |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 1316 - 1595 °C Show Material materials with Melting point of 1316 - 1595 °C | Typical for Nickel Steel | |
Specific heat capacity | 23.0 °C | 456 J/(kg·K) Show Material materials with Specific heat capacity of 456 J/(kg·K) | Typical for Nickel Steel |
Thermal conductivity | 23.0 °C | 10 - 50 W/(m·K) Show Material materials with Thermal conductivity of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.72 - 0.78 % Show Material materials with Carbon of 0.72 - 0.78 % |
Chromium | 0.15 % Show Material materials with Chromium of 0.15 % |
Manganese | 0.3 - 0.5 % Show Material materials with Manganese of 0.3 - 0.5 % |
Molybdenum | 0.1 % Show Material materials with Molybdenum of 0.1 % |
Nickel | 1.8 - 2.1 % Show Material materials with Nickel of 1.8 - 2.1 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.15 - 0.35 % Show Material materials with Silicon of 0.15 - 0.35 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |
Do you have a technical question or need more information about this material?